Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 2.063 g/cc | 2.063 g/cc | Woven Density |
Saint-Gobain Chemlam® 3320 Multi-plied, Flexible, Non-porous Fluoropolymer Laminated Composite Description: Chemlam® Ultra® is the trademark for the Chemfab® family of multi-plied, flexible, non-porous fluoropolymer laminated composites that combine the feature of multi-layer fluorop.. |