Polymer Property : Specific Gravity = 2.025 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 2.025 g/cc
2.025 g/cc
Woven Density
Saint-Gobain Chemlam® 6 Value Industrial Laminate
Description: The Chemlam® series is the Chemfab® value line of industrial laminates. Chemlam® composites features uniform thickness, multi-layer cast PTFE films laminated to fiber glass rei..
Specific Gravity 2.025 g/cc
2.025 g/cc
Woven Density
Saint-Gobain Chemlam® TR6 Value Industrial Laminate
Description: The Chemlam® series is the Chemfab® value line of industrial laminates. Chemlam® composites features uniform thickness, multi-layer cast PTFE films laminated to fiber glass rei..