Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 19.3 g/cc | 19.3 g/cc | Calculated |
Plansee S-WVMW Aluminum-potassium Silicate-doped tungsten Applications: anode materials - rod greater than 30 mm in diameter for short-arc lampsInformation provided by Plansee. |
|||
Specific Gravity | 19.3 g/cc | 19.3 g/cc | Calculated |
Plansee W-NS Potassium-doped Tungsten Doping tungsten with 60 to 65 ppm potassium produces an elongated stacked microstructure, yielding useful characteristics in wire products.Characteristics:Good creep resistanceGood high temperature .. |
|||
Specific Gravity | 19.3 g/cc | 19.3 g/cc | Calculated |
Plansee WVM Potassium-doped Tungsten Doping tungsten with potassium and subjecting the material to a highly orientation-dependant cold working produces a stacked microstructure, yielding useful characteristics in wire and rod products.. |
|||
Specific Gravity | 19.3 g/cc | 19.3 g/cc | Calculated |
Plansee WVMW Aluminum-potassium Silicate-doped tungsten Typical Application: anode materials - rod with diameter greater than 15 mm, for short-arc lampsInformation provided by Plansee. |