Polymer Property : Specific Gravity = 19.1 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 19.1 g/cc
19.1 g/cc
Calculated
Plansee WL15 Lanthanum Oxide-doped Tungsten
Tungsten alloy suitable for use as ion sources, lamp electrodes and welding electrodes.Characteristics (compared to pure tungsten):Improved creep resistanceHigher recrystallization temperatureMachin..