Physical Properties Metric English Comments
Specific Gravity 18.5 g/cc
18.5 g/cc
Plansee DENSIMET® D185 Tungsten-Nickel-Iron Alloy
Characteristics:Easy processingHigh densityPrecision forming and machiningHigh ductilityHigh strength100 % impermeableTypical Applications:Balancing weights in motors and drive componentsVibration d..