Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 17.6 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 17.6 g/cc
17.6 g/cc
Plansee DENAL® 910 179 20 Tungsten-Nickel-Iron-Cobalt Alloy
Characteristics:exceptionally stronghigh densityoutstanding mechanical damping capabilitiesHigh absorption of X-ray and gamma radiationInformation provided by Plansee.
Specific Gravity 17.6 g/cc
17.6 g/cc
Plansee DENAL® 920 159 20 Tungsten-Nickel-Iron-Cobalt Alloy
Characteristics:exceptionally stronghigh densityoutstanding mechanical damping capabilitiesHigh absorption of X-ray and gamma radiationInformation provided by Plansee.
Specific Gravity 17.6 g/cc
17.6 g/cc
Plansee DENAL® 920 60 20 Tungsten-Nickel-Iron-Cobalt Alloy
Characteristics:exceptionally stronghigh densityoutstanding mechanical damping capabilitiesHigh absorption of X-ray and gamma radiationInformation provided by Plansee.
Specific Gravity 17.6 g/cc
17.6 g/cc
Plansee DENSIMET® D176 Tungsten-Nickel-Iron Alloy
Characteristics:Easy processingHigh densityPrecision forming and machiningHigh ductilityHigh strength100 % impermeableTypical Applications:Balancing weights in motors and drive componentsVibration d..
Specific Gravity 17.6 g/cc
17.6 g/cc
Plansee INERMET® IT176 Tungsten-Nickel-Copper Alloy
Characteristics:Non-MagneticEasy processingHigh densityPrecision forming and machiningHigh ductilityHigh strength100 % impermeableTypical Applications:Balancing weights in motors and drive component..