Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 17.0 g/cc | 17.0 g/cc | |
Plansee DENSIMET® D170 Tungsten-Nickel-Iron Alloy Characteristics:Easy processingHigh densityPrecision forming and machiningHigh ductilityHigh strength100 % impermeableTypical Applications:Balancing weights in motors and drive componentsVibration d.. |
|||
Specific Gravity | 17.0 g/cc | 17.0 g/cc | |
Plansee INERMET® IT170 Tungsten-Nickel-Copper Alloy Characteristics:Non-MagneticEasy processingHigh densityPrecision forming and machiningHigh ductilityHigh strength100 % impermeableTypical Applications:Balancing weights in motors and drive component.. |