Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 16.87 g/cc | 16.87 g/cc | calculated |
Plansee Ta10W Tantalum-Tungsten 10 Alloy Tantalum-Tungsten alloys possess good mechanical properties and excellent corrosion resistance. Ta10W is stronger than pure tantalum, yet it remains easy to work at high temperatures, up to 1 600 °.. |