Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 12.0 g/cc | 12.0 g/cc | Calculated |
Plansee MW20 Molybdenum-Tungsten Characteristics:Improved high temperature properties when compared to pure tungstenImproved corrosion resistance compared to pure tungstenEnhanced etchabilityApplications:Manufacture of ZincGlass In.. |