Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.97 g/cc | 1.97 g/cc | |
Rogers Corporation Bisco® EC-2130 Conductive Silicone Base Polymer: SiliconeFiller: Nickel-GraphiteApplications: Silicone EMI ShieldsThickness: 0.063 inches and 0.125 inchesInformation provided by Rogers Corporation. |
|||
Specific Gravity | 1.97 g/cc | 1.97 g/cc | ASTM D-792 |
Glastic GLASTHERM HT200 Insulation Sheet HT200 features:High Hot Compressive StrengthLow Thermal ConductivityOil and Moisture ResistantReduces Heat LossHelps Control TemperatureFaster Mold StartupDesigned for reducing heat losses from plas.. |
|||
Specific Gravity | 1.97 g/cc | 1.97 g/cc | ASTM D297 |
Greene Tweed CHEMRAZ® 605 Perfluoroelastomer Chemraz® 605, a perfluoroelastomer, is ideally suited for challenging fluid handling applications. A high temperature compound with superior compression set resistance, physical properties and e.. |
|||
Specific Gravity | 1.97 - 2.03 g/cc | 1.97 - 2.03 g/cc | ASTM D 792 |
Karina 10/92-RG-GE (CS) White Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.97 g/cc | 1.97 g/cc | Saturated Solution |
Indium Corp. InCl3 Indium Trichloride Indium Trichloride is a white, odorless and highly deliquescent powder. Its particles are flake shaped and highly soluble in water and mineral acids. It is used as a starting chemical for the synt.. |
|||
Specific Gravity | 1.97 g/cc | 1.97 g/cc | ASTM D297 |
Greene Tweed CHEMRAZ® 600 Perfluoroelastomer Chemraz® 600, a perfluoroelastomer, works well in both high and low temperatures. It is capable of withstanding temperatures raging from -4°F to 500°F (-20°C to 260°C). Additionally.. |
|||
Specific Gravity | 1.97 g/cc | 1.97 g/cc | ASTM D792 |
PolyOne Syncure™ V0064G RoHS Polyethylene, Crosslinked (XLPE) Available as Flame Retardant Catalyst Masterbatch component for PolyOne Syncure System.Gel, Torque, Dispersion, and Oven Aging were measured on a 100 phr S1027A / 66.7 phr V0064G Syncure System. Cur.. |