Polymer Property : Specific Gravity = 1.875 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.875 - 3.125 g/cc
1.875 - 3.125 g/cc
ASTM D792
Parker Chomerics Tecknit Consil®-R 857 Pure Silver-Filled Silicone Elastomer
Description: CONSIL-R 857 provides similar properties as 856, with a high durometerTypical Applications: CONSIL-R is designed for use in low to moderate pressure applicationsInformation provided by ..
Specific Gravity 1.875 g/cc

@Temperature 20.0 °C
1.875 g/cc

@Temperature 68.0 °F
Indium Corp. Germanium Corporation® GeCl4 Germanium Tetrachloride
Germanium tetrachloride is a colorless liquid. It is used as an intermediate in the production of purified germanium dioxide and germanium metal, but more predominantly used as a reagent in fiber o..