Physical Properties Metric English Comments
Specific Gravity 1.70 - 1.86 g/cc
1.70 - 1.86 g/cc
ASTM D792
Daikin NEOFLON EP-521 ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
Specific Gravity 1.70 - 1.86 g/cc
1.70 - 1.86 g/cc
ASTM D792
Daikin NEOFLON EP-610 ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
Specific Gravity 1.70 - 1.86 g/cc
1.70 - 1.86 g/cc
ASTM D792
Daikin NEOFLON EP-610AS ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
Specific Gravity 1.70 - 1.86 g/cc
1.70 - 1.86 g/cc
ASTM D792
Daikin NEOFLON EP-620 ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
Specific Gravity 1.70 - 1.86 g/cc
1.70 - 1.86 g/cc
ASTM D792
Daikin NEOFLON EP-541 ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..