Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.716 g/cc | 1.716 g/cc | Calculated |
PolyOne Aquamix™ 142 Latex Storage Stability: In excess of 6 months when stored under proper conditions in original sealed container. Keep from freezing. Water lost by evaporation can adversely affect viscosity, dispersabilit.. |