Specific Gravity 1.65 - 1.69 g/cc
1.65 - 1.69 g/cc
ASTM D-792
Axiall 02540 Plenum Flexible PVC
Non-lead stabilized Category 3 plenum jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.