Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.642 g/cc | 1.642 g/cc | ASTM D792 |
PolyOne Lubri-Tech™ AT-20GB/15T Acetal-Copolymer, Glass Bead Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Bead FilledPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |