Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.523 g/cc | 1.523 g/cc | ASTM D792 |
PolyOne Lubri-Tech™ PS-30GF/02S Polybutylene Terephthalate (PBT), Glass Filled, PTFE/Silicone Lubricated
(dis Description/Features:Glass Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |