Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.495 g/cc | 1.495 g/cc | ASTM D792 |
PolyOne Lubri-Tech™ PI-30CF/15T Polyetherimide (PEI), Carbon Fiber Reinforced, PTFE Lubricated
(discontinued Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |