Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.482 g/cc | 1.482 g/cc | ASTM D792 |
PolyOne Edgetek® ATH-20CF/000 Acetal-Homopolymer, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedElectrically ConductivePolyOne First ChoiceInformation provided by PolyOne Corporation. |