Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.478 g/cc | 1.478 g/cc | ASTM D792 |
PolyOne Lubri-Tech™ AT-10GF-10KV/000 Acetal-Copolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedAramid Fiber ReinforcedInformation provided by PolyOne Corporation. |