Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.435 g/cc | 1.435 g/cc | ASTM D792 |
PolyOne Lubri-Tech™ AT-000/5T Black Acetal-Copolymer, PTFE Lubricated
(discontinued **) Preliminary DataDescription/Features:PTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Specific Gravity | 1.435 g/cc | 1.435 g/cc | ASTM D792 |
PolyOne Lubri-Tech™ ATH-000/5T Acetal-Homopolymer, PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedInformation provided by PolyOne Corporation. |