Polymer Property : Specific Gravity = 1.427 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.427 g/cc
1.427 g/cc
ASTM D792
PolyOne Edgetek® PE-30MC-20TC/000 High Density Polyethylene (HDPE), Talc Filled  (discontinued **)
Description/Features:Mica FilledTalc FilledInformation provided by PolyOne Corporation.