Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.426 g/cc | 1.426 g/cc | ASTM D792 |
PolyOne Edgetek® PS-30CF/000 Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |