Polymer Property : Specific Gravity = 1.393 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.393 g/cc
1.393 g/cc
ASTM D792
PolyOne Lubri-Tech™ PK-5GP/7T Polyetheretherketone (PEEK), PTFE Lubricated  (discontinued **)
Description/Features:Graphite LubricatedPTFE LubricatedInformation provided by PolyOne Corporation.