Physical Properties Metric English Comments
Specific Gravity 1.365 g/cc
1.365 g/cc
ASTM D792
LG Chemical LUMID EG2309B(W) PA66+GF30%, Chemical Resistance(CaCl2, Ethylene Glycol)
Feature: Injection Molding, PA66+GF30%, Chemical Resistance(CaCl2, Ethylene Glycol)Application: Radiator Tank, Intercooler TankCAS No. 32131-17-2, 65997-17-3 and 9010-79-9Information provided by LG ..
Specific Gravity 1.365 g/cc
1.365 g/cc
ISO 1183
Lanxess Durethan® BKV 30 G W1 901317 Nylon 6, Glass Fiber Reinforced
PA 6, 30% glass fibers, injection molding, weather stabilizedInformation provided by LANXESS.