Physical Properties Metric English Comments
Specific Gravity 1.353 g/cc
1.353 g/cc
ASTM D-792
Axiall 3020 Rigid PVC, Extrusion
Georgia Gulf 3020 is a base for use of wood flour up to 40 percent. Impact strength and toughnessFlame retardantChemical resistanceDimensional stabilityInformation provided by Georgia GulfGeorgia G..