Polymer Property : Specific Gravity = 1.247 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.247 g/cc
1.247 g/cc
ASTM D792
PolyOne Lubri-Tech™ BB-10GF/5T PC/ABS Blend, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.