Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.219 g/cc @Temperature 25.0 °C |
1.219 g/cc @Temperature 77.0 °F |
|
Dow Corning SLYGARD® HVIC + This one-part silicone coating is designed for high-voltage insulators, instrument transformers and other high-voltage devices where surface contamination causes insulation problems. SYLGARD HVIC+ i.. |