Polymer Property : Specific Gravity = 1.169 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.169 g/cc
1.169 g/cc
ISO 1183
Lanxess Durethan® BKV 215 H2.0 DUS008 901510 Nylon 6, Impact Modified
PA 6, 15% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Specific Gravity 1.169 g/cc
1.169 g/cc
ISO 1183
Lanxess Durethan® DP A 30 S FN30 DUS025 000000 Nylon 66
PA 66, non-reinforced, injection molding, halogen free flame retardant improved flowabilityInformation provided by LANXESS.
Specific Gravity 1.169 g/cc
1.169 g/cc
ISO 1183
Lanxess Durethan® A 30 S FN31 000000 Nylon 66, Flame Retardant
PA 66, non-reinforced, injection molding, halogen-free flame retardant, improved flowabilityInformation provided by LANXESS.