Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.156 g/cc @Temperature 25.0 °C |
1.156 g/cc @Temperature 77.0 °F |
|
Dow Corning 3074 INTERMEDIATE Reactive silicone intermediate for coil coatings, appliance finishes and other finishes where improved heat or weathering resistance is needed. Typically reacted with saturated polyesters to form si.. |