Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.155 g/cc | 1.155 g/cc | 15.6°C |
ExxonMobil Mobil Pyrogard 53 Mobil Pyrogard 53 is a high performance phosphate ester synthetic fluid designed to replace petroleum-based oils in hydraulic applications where operating conditions preclude the use of combustible .. |
|||