Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.125 g/cc | 1.125 g/cc | ASTM D792 |
Fiberfil® J-62/30/E8 Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Specific Gravity | 1.125 g/cc | 1.125 g/cc | ASTM D792 |
Fiberfil® J-62/30/E Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |