Polymer Property : Specific Gravity = 1.107 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.107 g/cc
1.107 g/cc
Chesterton OPTICOOLâ„¢ 970 Synthetic Fluid
Description: OPTICOOL 970 is a high performance, low maintenance synthetic fluids. OPTICOOL 970 formulation is DEA and Boron free and offers superior lubricity, corrosion inhibition, extreme pressur..