Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.094 g/cc | 1.094 g/cc | ASTM D792 |
Trelleborg Emerson & Cuming EP651 Patch Paste Density matched brown adhesive for use with EP650 and TB650All information provided by Trelleborg Emerson & Cuming |