Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.069 - 1.073 g/cc
1.069 - 1.073 g/cc
D2020
Oceanchem Group Triethyl Phosphate (TEP)
Molecular Formula: (CH3CH2O)3POCas No.: 78-51-3Use: Flammable inhibitor of rubber and plastic; raw material for pesticide, hardener and stabilizer of resin.Characteristics: It can dissolve in water ..