Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.025 g/cc | 1.025 g/cc | |
Northstar Polymers PBD-025 Curing Agent Information provided by Northstar Polymers. |
|||
Specific Gravity | 1.025 g/cc | 1.025 g/cc | |
Struktol VLB 618 Processing Additive Blend of fatty acid esters. STRUKTOL® VLB-618 is manufactured from high quality vegetable fatty acids.Applications: STRUKTOL® VLB-618 is the vegetable version of VLB-602 and is a very compatib.. |
|||
Specific Gravity | 1.025 g/cc @Temperature 25.0 °C |
1.025 g/cc @Temperature 77.0 °F |
|
Dow Corning 2-1912 FLUID Blend of polydimethylsiloxane and high molecular weight silicone resin. Reactive silicone fluids used for silica treatment.Information provided by Dow Corning |