Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.013 g/cc @Temperature 25.0 °C |
1.013 g/cc @Temperature 77.0 °F |
|
Dow Corning SYL-OFF® 2-7131 FAST CURE ADDITIVE Syl-Off® 7131 Fast Cure Additive is a 100% active solids organo-silicone compound. This product is recommended for use as a fast cure additive when used in conjunction with an organo-tin functional.. |