Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.006 g/cc | 1.006 g/cc | |
Struktol V-PEDS Processing Additive Fatty acid esterTypical Applications: STRUKTOL® V-PEDS has both internal and external lubricant characteristics. It can be used in calendaring, extrusion and injection molding applications. It al.. |