Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.959 - 0.969 g/cc @Temperature 25.0 °C |
0.959 - 0.969 g/cc @Temperature 77.0 °F |
ASTM D4052 |
PolyOne Synplast™ 701P-N Di (C7-C11 Alkyl) Phthalate Linear alkyl phthalate esterInformation provided by PolyOne |