Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.953 - 0.959 g/cc @Temperature 25.0 °C |
0.953 - 0.959 g/cc @Temperature 77.0 °F |
ASTM D4052 |
PolyOne Synplast™ 901P-N Di (Nonyl, Decyl, Undecyl) Phthalate Linear phthalate esterInformation provided by PolyOne |
|||
Specific Gravity | 0.953 - 0.959 g/cc @Temperature 25.0 °C |
0.953 - 0.959 g/cc @Temperature 77.0 °F |
ASTM D4052 |
PolyOne Synplast™ 901P-E Di (Nonyl, Decyl, Undecyl) Phthalate Linear phthalate esterNote: Contains 0.1 - 0.15 wt% 1,1,3-Tris (2-methyl-4-hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne |