Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.931 g/cc | 0.931 g/cc | ASTM D1505/D792 |
Braskem TS9022 Blown Film Extrusion Low Density Polyethylene Films for automatic overwrap packaging of hygiene markets. Typical applications are toilet tissue, kitchen paper and napkin (paper product) overwrap. Films which require good optical properties al.. |