Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.914 - 0.916 g/cc | 0.914 - 0.916 g/cc | ASTM D1505 |
LG Chemical SEETEC ST408 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Excellent puncture resistance, tear strength. Excellent sealing and optical properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplica.. |