Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.891 g/cc | 0.891 g/cc | 15°C; ASTM D1298 |
ExxonMobil 417 Mobilmet 400 Series Mobilmet 400 Series products are high-performance multi-purpose cutting oils. They are chlorine-free, non-staining and non-corrosive. They are designed for light to moderate duty cutting operation.. |
|||
Specific Gravity | 0.891 g/cc | 0.891 g/cc | 15.6°C; ASTM D1298 |
ExxonMobil Teresstic 150 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Specific Gravity | 0.891 g/cc | 0.891 g/cc | 15°C; ASTM D1298 |
ExxonMobil 417 Mobilmet 400 Series Mobilmet 400 Series products are high-performance multi-purpose cutting oils. They are chlorine-free, non-staining and non-corrosive. They are designed for light to moderate duty cutting operation.. |
|||
Specific Gravity | 0.891 g/cc | 0.891 g/cc | 15.6°C; ASTM D1298 |
ExxonMobil Teresstic 150 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |