Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.883 g/cc | 0.883 g/cc | 15°C; ASTM D1298 |
ExxonMobil Mobil Vactra 2 The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a.. |
|||
Specific Gravity | 0.883 g/cc | 0.883 g/cc | 60°F |
ConocoPhillips Conoco® El Mar® Ashless Heavy Duty Oil, SAE Viscosity Grade 30 Conoco® El Mar Ashless Heavy Duty is a high-quality, ashless, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately turbocharged 2-stroke cycle natural gas engi.. |
|||
Specific Gravity | 0.883 g/cc | 0.883 g/cc | 15°C; ASTM D1298 |
ExxonMobil Mobil Vactra 2 The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a.. |
|||
Specific Gravity | 0.883 g/cc | 0.883 g/cc | 60°F |
ConocoPhillips Conoco® El Mar® Ashless Supreme Oil, SAE Viscosity Grade 30 Conoco® El Mar Ashless Supreme is a premium quality, ashless, dispersant-detergent gas engine oil designed for use in naturally aspirated and turbocharged 2-stroke cycle natural gas engines. Engine.. |