Polymer Property : Specific Gravity = 0.8772 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.8772 g/cc
0.8772 g/cc
ExxonMobil Mobiltherm 43
Mobiltherm 43 is a formulated paraffinic type fluid designed for closed heat transfer systems operating at higher bulk temperatures including demanding open systems.  It has a high specific heat an..
Specific Gravity 0.8772 g/cc
0.8772 g/cc
ExxonMobil Mobiltherm 43
Mobiltherm 43 is a formulated paraffinic type fluid designed for closed heat transfer systems operating at higher bulk temperatures including demanding open systems.  It has a high specific heat an..