Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.864 g/cc | 0.864 g/cc | ASTM D1505 |
ExxonMobil Exact™ 9361 Ethylene-based Plastomer Resin Product Description: Exact 9361 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P.. |
|||