Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.8545 g/cc | 0.8545 g/cc | |
ChevronTexaco ParaLux® 1001 Paraffinic Process Oil FeaturesPARALUX is produced using an all-hydroprocessing route which transforms the molecular structure of undesirable aromatics into highly desirable saturates. This produces a process oil with sup.. |
|||
Specific Gravity | 0.8545 g/cc | 0.8545 g/cc | |
ChevronTexaco ParaLux® 1001R Process Oil FeaturesPARALUX is produced using an all-hydroprocessing route which transforms the molecular structure of undesirable aromatics into highly desirable saturates. This produces a process oil with sup.. |