Polymer Property : Specific Gravity = 0.821 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.821 g/cc
0.821 g/cc
ConocoPhillips Syncon® 22 Synthetic AW Hydraulic Fluid 22
Syncon AW Hydraulic Fluid is a premium quality, synthetic antiwear hydraulic fluid developed for use in industrial and mobile equipment operating at extreme temperatures. It is particularly recommen..