Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.799 g/cc | 0.799 g/cc | 15°C; ASTM D4052 |
ExxonMobil Mobil Synturion 6 Mobil Synturion 6 is a premium-quality, synthetic-base fluid specially formulated to meet the demanding lubrication and cooling requirements of mechanical seals --and to maximize seal life. The supe.. |
|||
Specific Gravity | 0.799 g/cc | 0.799 g/cc | 15°C; ASTM D4052 |
ExxonMobil Mobil Synturion 6 Mobil Synturion 6 is a premium-quality, synthetic-base fluid specially formulated to meet the demanding lubrication and cooling requirements of mechanical seals --and to maximize seal life. The supe.. |