Polymer Property : Specific Gravity = 0.786 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.786 g/cc
0.786 g/cc
ASTM D1298
LG Chemical HP-IPA ISOPROPYL ALCOHOL
Features: IPA is produced by the direct propylene hydration process. IPA meets the diverse needs from solvent industry. Our division has been a stable supplier of raw materials for related industrie..
Specific Gravity 0.786 g/cc
0.786 g/cc
ASTM D1298
LG Chemical IPA ISOPROPYL ALCOHOL
Features: IPA is produced by the direct propylene hydration process. IPA meets the diverse needs from solvent industry. Our division has been a stable supplier of raw materials for related industrie..