Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.729 g/cc | 0.729 g/cc | 200°C |
ChevronTexaco 22 Heat Transfer Oil FeaturesChevron Heat Transfer Oils are mineral-type transfer oils for use in secondary or indirect heating systems. They are formulated with ISOSYN® base stocks. Chevron Heat Transfer Oils are nont.. |